Ceradel Frit C 1253

High expansion frit, Fritte boro-alcaline sans plomb

Alternate Names: Fritte C1253, Fritte C 1253, Ceradel Frit 1253

OxideAnalysisFormula
BaO2.54%0.050
CaO3.91%0.212
Na2O13.37%0.657
ZnO2.16%0.081
Al2O36.43%0.192
B2O321.72%0.950
SiO249.86%2.526
Oxide Weight304.43
Formula Weight304.43
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 99x10-7 (20/300C)
GSPT - Frit Softening Point 880-920C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceradel Frit C 1253" descrip="High expansion frit, Fritte boro-alcaline sans plomb" searchkey="Fritte C1253, Fritte C 1253, Ceradel Frit 1253" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.540" tolerance="10"/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.910" tolerance=".5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.370" tolerance="3"/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.160" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.430" tolerance="15"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.720" tolerance="10"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.860" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved