Ceradel Frit C 1252

Fritte borocalcique sans plomb

Alternate Names: Fritte C1252, Fritte C 1252, Ceradel Frit 1252

OxideAnalysisFormula
CaO15.21%0.820
K2O2.80%0.090
Na2O1.85%0.090
Al2O313.83%0.410
B2O322.57%0.981
SiO243.73%2.200
Oxide Weight302.37
Formula Weight302.37
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 58x10-7 (20/300C)
GSPT - Frit Softening Point 900-980C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceradel Frit C 1252" descrip="Fritte borocalcique sans plomb" searchkey="Fritte C1252, Fritte C 1252, Ceradel Frit 1252" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="15.210" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.850" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.830" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="22.570" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.730" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved