Ceradel Frit C 1251

Lead monosilicate frit, Monosilicate de plomb

Alternate Names: C1251 Fritte, C 1251 Fritte, Ceradel Frit 1251

OxideAnalysisFormula
PbO78.79%1.000
SiO221.21%1.000
Oxide Weight283.28
Formula Weight283.28
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 83x10-7 (20-300C)
GSPT - Frit Softening Point 900-1100C

This analysis is guessed, the manufacturer calls it a lead monosilicate and provides the approximate chemistry of (SiO2 - 15-40%, PbO 60-100%. However since the lead monosilicate analysis is universally 1:1 lead:silica that is what we have assigned here.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceradel Frit C 1251" descrip="Lead monosilicate frit, Monosilicate de plomb" searchkey="C1251 Fritte, C 1251 Fritte, Ceradel Frit 1251" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="78.790" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="21.210" tolerance=""/> </oxides> </material>