Ceradel Frit 3110

High sodium, low boron/alumina frit

Alternate Names: Ceradel Fritte 3110

OxideAnalysisFormula
CaO6.50%0.295
K2O2.50%0.068
Na2O15.50%0.637
Al2O34.00%0.100
B2O32.50%0.092
SiO269.00%2.926
Oxide Weight254.84
Formula Weight254.84
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 100.8 (10-7/C 20/300C)
MLRG - Frit Melting Range (C) 1000-1300C

Ceradel provides a slightly different chemistry for this than Ferro does for its 3110 standard formulation.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ceradel Frit 3110" descrip="High sodium, low boron/alumina frit" searchkey="Ceradel Fritte 3110" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved