Cendre de lavande

OxideAnalysisFormula
CaO29.26%0.607
MgO5.66%0.164
K2O14.71%0.182
Na2O0.39%0.007
P2O54.88%0.040
TiO20.21%0.003
Al2O33.54%0.040
SiO216.59%0.321
Fe2O31.26%0.009
LOI20.30
Oxide Weight89.07
Formula Weight111.76
If this formula is not unified correctly please contact us.

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Cendre de lavande" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="29.260" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="5.660" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="14.710" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.390" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="4.880" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.210" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.540" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="16.590" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.260" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="20.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved