CDI Ball Clay

Oxide Analysis Formula
CaO 0.30% 0.02
K2O 1.20% 0.05
MgO 0.30% 0.03
Na2O 0.20% 0.01
TiO2 1.50% 0.07
Al2O3 28.10% 1.00
SiO2 57.40% 3.47
Fe2O3 0.80% 0.02
LOI10.20%
Oxide Weight 325.96
Formula Weight 362.99

Notes

This is sold by Chemical Distributors Inc. to be used in a 50:50 mix with Texas Pioneer Talc.
It is a mixture of 75% SGP Ball Clay and 25% OM#4 Ball Clay.

Related Information

Links

Materials Ball Clay
Suppliers K&T Clays
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved