Calcined Missouri Fireclay

OxideAnalysisFormula
CaO0.24%0.010
MgO0.29%0.017
K2O1.12%0.027
Na2O0.10%0.004
P2O50.12%0.002
TiO22.50%0.072
Al2O344.19%1.000
SiO250.34%1.933
Fe2O30.99%0.014
SO30.07
Oxide Weight230.57
Formula Weight230.73
If this formula is not unified correctly please contact us.

A very high-melting zero-plasticity material used in the refractories industry to make castables, brick, ramming and gunning mixes, mortars and potters grog. This material is fairly clean (speck free) and also answers a common need for stoneware clay bodies: An economical addition that will make the body more refractory but not add to its plasticity and produce drying problems.

It is fairly coarse and available in many particle sizes, the finest of which is 5-10% retained on a 70 mesh screen. Special sizes are available for custom orders.

The company calcines the materials and makes many grades of aggregate products.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Calcined Missouri Fireclay" descrip="" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.240" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.290" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.120" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.120" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="2.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="44.190" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.340" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.990" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO3" name="Sulfur Trioxide" percent="0.070" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved