BPS Lead Bisilicate

Lead alumina bilsilicate frit

OxideAnalysisFormula
PbO64.97%1.000
Al2O32.67%0.090
SiO232.36%1.850
Oxide Weight343.54
Formula Weight343.54
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="BPS Lead Bisilicate" descrip="Lead alumina bilsilicate frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="64.970" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.670" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.360" tolerance=""/> </oxides> </material>