BPS Cornish Stone

OxideAnalysisFormula
CaO1.48%0.193
MgO0.13%0.024
K2O4.51%0.349
Na2O3.48%0.409
P2O50.47%0.024
TiO20.06%0.006
Al2O315.49%1.106
SiO274.22%8.994
Fe2O30.12%0.006
Oxide Weight728.33
Formula Weight728.33
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="BPS Cornish Stone" descrip="" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.488" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.135" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.517" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.480" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.475" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.064" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="15.493" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="74.220" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.129" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved