BPS Calcium Borate Frit

Calcium Borate Frit

OxideAnalysisFormula
CaO26.60%0.980
MgO0.19%0.010
K2O0.45%0.010
Al2O34.88%0.099
B2O350.01%1.485
SiO217.85%0.614
Oxide Weight206.68
Formula Weight206.68
If this formula is not unified correctly please contact us.

Chemistry similar to colemanite


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="BPS Calcium Borate Frit" descrip="Calcium Borate Frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="26.606" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.193" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.451" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.886" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="50.013" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="17.850" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved