Black & Tan Clay

Originally from HC Spinks in 1970s

Alternate Names: Blank and Tan Clay, Ball & Tan Ball Clay

OxideAnalysisFormula
CaO0.42%0.035
MgO0.37%0.043
K2O1.01%0.051
Na2O0.43%0.033
TiO20.36%0.021
Al2O321.65%1.000
SiO264.75%5.076
Fe2O31.60%0.047
LOI9.39
SO30.08
Oxide Weight426.80
Formula Weight471.44
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Black & Tan Clay" descrip="Originally from HC Spinks in 1970s" searchkey="Blank and Tan Clay, Ball & Tan Ball Clay" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.420" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.370" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.010" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.430" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.360" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="21.650" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="64.750" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="9.390" tolerance=""/> <volatile symbol="SO3" name="Sulfur Trioxide" percent="0.080" tolerance=""/> </volatiles> </material>