Bentonite NZ14

Imerys tableware material

Alternate Names: NZ-14 Bentonite

OxideAnalysisFormula
CaO1.50%0.158
MgO3.40%0.499
K2O0.30%0.019
Na2O3.40%0.324
TiO20.10%0.007
Al2O313.00%0.754
SiO270.00%6.887
Fe2O31.30%0.048
LOI5.70
Oxide Weight549.88
Formula Weight583.11
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Bentonite NZ14" descrip="Imerys tableware material" searchkey="NZ-14 Bentonite" loi="0.00" casnumber="52623-66-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.400" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.300" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="5.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved