Bentolite B

White burning processed bentonite

Alternate Names: Bentolite BC, Mineral Colloid BP

OxideAnalysisFormula
CaO0.70%0.118
MgO2.40%0.562
Na2O2.10%0.320
TiO20.10%0.012
Al2O317.10%1.583
SiO262.90%9.883
Fe2O34.80%0.283
LOI9.50
Oxide Weight850.79
Formula Weight940.10
If this formula is not unified correctly please contact us.

A high purity montmorillonite refined to meet the thixotropic needs of water-based systems where high viscosity is required without the demand for whiteness (it has a much higher iron content that the other bentonlite products). Mineral Colloid® BP provides suspension stability and viscosity control. It is targetted at the Home Care and Personal Care markets.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Bentolite B" descrip="White burning processed bentonite" searchkey="Bentolite BC, Mineral Colloid BP" loi="0.00" casnumber="52623-66-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.700" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="4.800" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="9.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved