Barium Feldspar

Formula: BaAl2Si2O8
Alternate Names: Celsian

OxideAnalysisFormula
BaO40.84%1.000
Al2O327.16%1.000
SiO232.01%1.999
Oxide Weight375.40
Formula Weight375.40
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Barium Feldspar" descrip="" searchkey="Celsian" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="40.840" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="27.160" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.010" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved