Arcola Slip

FROM AUTUMN DOWNEY, SASK.

OxideAnalysisFormula
CaO8.40%1.469
MgO4.20%1.022
K2O2.10%0.219
Na2O1.30%0.206
P2O50.20%0.014
TiO20.60%0.074
Al2O310.40%1.000
SiO254.92%8.962
Fe2O33.80%0.233
MnO0.10%0.014
LOI13.00
Oxide Weight843.66
Formula Weight969.72
If this formula is not unified correctly please contact us.

Autumn Downey published this on Clayart. It is a local clay she uses to make glazes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Arcola Slip" descrip="FROM AUTUMN DOWNEY, SASK." searchkey="" loi="13.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.400" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="4.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.300" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="10.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.920" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="3.800" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="13.000" tolerance=""/> </volatiles> </material>