Arcilla Revolucion II (Cuba)

Cuban clay

OxideAnalysisFormula
CaO1.40%0.081
MgO2.00%0.160
K2O1.30%0.045
Na2O0.25%0.013
TiO20.71%0.029
Al2O331.60%1.000
SiO248.70%2.616
Fe2O33.01%0.061
LOI12.30
Oxide Weight287.18
Formula Weight327.46
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Arcilla Revolucion II (Cuba)" descrip="Cuban clay" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.400" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.250" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.710" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="31.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="3.010" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="12.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved