Formula: Li.AlF.PO4
| If this formula is not unified correctly please contact us. |
DENS - Density (Specific Gravity) | 3.00 |
HMOH - Hardness (Moh) | 6.0 |
GSPT - Frit Softening Point | 1100C D |
This material requires oxidation if used as a glaze material to minimize blisters due to products of decomposition.
From Watkins Minerals in Wichita Falls, TX.
Out Bound Links
A fluorophosphate mineral.