ABC Colemanite

California colemanite

OxideAnalysisFormula
CaO29.60%0.966
MgO0.30%0.014
Na2O0.10%0.003
SrO1.00%0.018
Al2O30.20%0.004
B2O342.60%1.120
SiO20.60%0.018
Fe2O30.10%0.001
LOI25.50
Oxide Weight136.36
Formula Weight183.04
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="ABC Colemanite" descrip="California colemanite" searchkey="" loi="0.00" casnumber="1318-33-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="29.600" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="42.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="0.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="25.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved