A-3 Feldspar

potash feldspar

Alternate Names: A3 Feldspar, Kona A-3 Feldspar, Kona A3 Feldspar

OxideAnalysisFormula
CaO0.40%0.047
K2O7.51%0.527
Na2O4.00%0.426
Al2O316.30%1.056
SiO271.63%7.874
Fe2O30.07%0.003
LOI0.09
Oxide Weight660.04
Formula Weight660.63
If this formula is not unified correctly please contact us.

No longer available.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="A-3 Feldspar" descrip="potash feldspar" searchkey="A3 Feldspar, Kona A-3 Feldspar, Kona A3 Feldspar" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="7.510" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="71.630" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.070" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.090" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved