98 Mix

Low temperature very plastic iron stained clay

OxideAnalysisFormula
CaO0.70%0.118
MgO1.00%0.236
K2O3.00%0.302
Na2O2.20%0.337
P2O50.10%0.007
TiO20.60%0.071
Al2O313.90%1.294
SiO269.30%10.948
Fe2O32.80%0.166
LOI5.20
Oxide Weight888.66
Formula Weight937.40
If this formula is not unified correctly please contact us.

Lording Labs analysis 2006 showed 15.6 Al2O3, 3.9 Fe2O3, 4.9 SO3, 64.9 SiO2, 3.4 LOI.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="98 Mix" descrip="Low temperature very plastic iron stained clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.700" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.200" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.900" tolerance="13.9"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.300" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.800" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="5.200" tolerance=""/> </volatiles> </material>