1D Sandy Stoneware

PR#1 D, Buff Burning Sandy Stoneware

OxideAnalysisFormula
CaO0.13%0.016
MgO0.38%0.066
K2O2.64%0.195
Na2O0.16%0.018
P2O50.02%0.001
TiO20.60%0.052
Al2O314.66%1.000
SiO275.38%8.727
Fe2O31.02%0.044
MnO0.01%0.001
LOI5.67
Oxide Weight660.98
Formula Weight700.71
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="1D Sandy Stoneware" descrip="PR#1 D, Buff Burning Sandy Stoneware" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.130" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.380" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.640" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.160" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.020" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="14.660" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="75.380" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.020" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.010" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="5.670" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved