1434 Kaolin

Ivory burning legacy kaolin

OxideAnalysisFormula
CaO0.50%0.023
TiO21.00%0.032
Al2O340.00%1.000
SiO244.00%1.867
Fe2O30.50%0.008
Cl13.25
Oxide Weight219.30
Formula Weight252.80
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="1434 Kaolin" descrip="Ivory burning legacy kaolin" searchkey="" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.500" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="40.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.500" tolerance=""/> </oxides> <volatiles> <volatile symbol="Cl" name="Chlorine Gas" percent="13.250" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved