Use Insight-live to substitute materials in a recipe

We will substitute wollastonite for whiting and a frit for Gerstley borate in G2571A while maintaining the chemistry of the original recipe.

A. Insight-live


Click here to watch this at youtube.com or click here to go to our Youtube channel

Colemanite and what its decrepitation does in glazes

Colemanite and what its decrepitation does in glazes

Decrepitation refers to a decomposition accompanied by scaling, delayering, even disintegration of the glaze layer. Moving rightward these glazes have increasing percentages of colemanite. At its worst (far right) the glaze is spattering off the sample and onto the kiln shelf. The others are crawling, first pulling away from the corners (far left) moving toward pulling away on the flat surfaces (center). Gerstley Borate and Ulexite, similar minerals, are far less likely to do this (but they have other serious issues also). A much better solution is to use frits to source the oxide B2O3 (easy to do in your account at Insight-live.com). Photos courtesy of Nigel Hicken.

In Bound Links

  • (Recipes) G2571A - Cone 10 Silky Dolomite Matte Base Glaze

    A cone 10R dolomite matte having a pleasant silky surface, it does not cutlery mark, stain or craze on common bodies

    2003-12-18 - A standard Plainsman Clays cone 10R dolomite matte glaze used for many years. Colorants and opacifiers can be added to create a wide range of beautifu...


By Tony Hansen




Feedback, Suggestions