Making ceramic glaze flow test balls

Making 10 gram balls of your glaze and firing them on 2in by 2in tiles is a great way to evaluate their flow, surface and susceptibility to defects.

B. Glazes


Click here to watch this at youtube.com or click here to go to our Youtube channel

I will show you how I make the balls. This test provides valuable information to help you compare and judge the suitability of glazes. You only need to make 100 grams of glaze in a zip lock bag to do this.