Insight-Live Meets a Silica Deprived Glaze Recipe

Using Insight-live I will demonstrate the surprising amount of silica some cone 6 base glazes that appear OK will accept and still melt well.

A. Insight-live


Click here to watch this at youtube.com or click here to go to our Youtube channel

This glossy ceramic glaze lacks SiO2 (detrimental to its hardness, leaching resistance, resistance to crazing). Let us see how much silica this glaze will accept!


By Tony Hansen




Feedback, Suggestions