BQ1000 - Plainsman Electric Bisque Firing Schedule
C04PLTP - Plainsman Typical Cone 04
C10RPL - Plainsman Cone 10R Firing
C6DHSC - Plainsman Cone 6 Slow Cool (Reactive glazes)
C6MSGL1 - Mastering Glazes Cone 6
C6PLST - Plainsman Cone 6 Electric Standard
FSCG1 - Shimbo Crystal Schedule 1
FSCGB1 - Bory 1 Fara Shimbo Crystalline Glaze
FSCGCL - Celestite
FSCGWM - Wollast-O-Matte Fara Shimbo Crystalline Glaze
FSCRGL - GC106 Base for Crystalline Glazes
FSHP1 - Shimbo Crystal Holding Pattern 1
FSHP2 - Shimbo Crystal Holding Pattern 2
FSHP3 - Shimbo Crystal Holding Pattern 3
FSNM5 - Fa's Number Five
PLC6CR - Cone 6 Crystal Glaze Plainsman
PLC6DS - Cone 6 Drop-and-Soak Firing Schedule
PLLFDS - Low Fire Drop-and-Hold

FSCRGL Firing Schedule

GC106 Base for Crystalline Glazes

Step °C °F Hold Time
1 100°C/hr to 200C  180°F/hr to 392F  0 2:02  
2 250°C/hr to 500C  450°F/hr to 932F  0 3:14  
3 500°C/hr to 1275C  900°F/hr to 2327F  0 4:47  
4 9999°C/hr to 1130C  17998°F/hr to 2066F  15min 5:03  
5 30°C/hr to 1075C  54°F/hr to 1967F  0 6:53  
Start temperature assumed: 25°C or 75°F

Links

Recipes GC - GC106 Base Fara Shimbo Crystalline Glaze
Cone 9-10 for brilliant colors
Typecodes Oxidation Firing

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved