Ravenscrag Cone 10R Talc Matte| Code | GR10-C |
| Modification Date | 2012-07-23 11:44:48 |
| Member of Group | RV 10 |
Recipe| Material | Amount | Units | +/- | *Stat |
| Ravenscrag Slip | 90.00 | kg | | |
| Talc | 10.00 | kg | | |
| | 100.00 | |
3-95
Pictures GR10-C Ravenscrag glaze on iron stoneware

GR10-C Ravenscrag glaze on grey stoneware.

|
The future of ceramic recipe, material and physical testing record keeping is here. Just pennies a day.
Maintain your recipes and materials on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Import existing material, recipe data.
- As many side-by-side recipes and/or materials as you want (chemistry is shown for all).
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, pictures with individual titles and descriptions, material links.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to materials, typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to recipe imports (later search by batch).
- Assign multiple typecodes to imported glaze and body batches (to classify) (search on these later).
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding recipe records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
- Import materials data in various formats or just use the thousands of built-in reference materials.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|
|