Ravenscrag Cone 10R Matte

CodeGR10-C
Modification Date2011-08-02 17:34:08
Member of GroupRV10

Recipe

MaterialAmountUnits+/-*Stat
Ravenscrag Slip90.00kg  
Talc10.00kg  
 100.00  