A3 Test| Code | L2001 |
| Modification Date | 2008-07-04 12:37:56 |
Recipe| Material | Amount | Units | +/- | *Stat |
| A3 | 100.00 | kg | | |
| | 100.00 | |
Test DataShrinkage/Absorption (SHAB)
Soluble Salts (SOLU)
Clay Water Content - Powder, Plastic (CLWC)| Sp |
WPOW |
POWW |
POWD |
WPUG |
PUGW |
PUGD |
| 1 |
4.5 |
|
|
23.1 |
|
|
Sieve Analysis 35-325 Wet (SIEV)| Sp |
TOT |
35M |
48M |
65M |
100M |
150M |
200M |
325M |
NOTE |
| 1 |
100 |
|
|
|
|
|
|
|
|
1-11
Out Bound Links
|
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|
|