Mineral: AsbestosNotes'Asbestos' is a generic term referring to a group of closely related fibrous magnesium silicate minerals. Tremolite is more distantly related and occurs in some talcs.
Its fibrous nature, very high melting temperature, resistance to chemical attack, low thermal and electrical conductivity have made asbestos valuable in many manufactured products. For example, asbestos fabrics were used for many years in clothing and structural products that required flame resistance and insulting properties. In ceramics, kilns were fitted with asbestos boards and modules, and buildings of all types have employed asbestos fireproofing products.
However since the public has become aware of the dangers of breathing in asbestos fibers industry has moved to find substitutes. In some cases excellent progress has been made. For example, man-made aluminum silicate fibers have been developed that can withstand very high temperatures and have extremely good insulating properties (e.g. these are used in gloves, clothing, kiln and furnace liners). In other cases it has been much more difficult to find substitutes. There have been moves to ban all asbestos use, but in most countries things have evolved into a climate of controlled use instead. One reason is that the materials employed as substitutes have been found to have significant hazards of their own. Out Bound Links
|
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|