FINE GROUND SODIUM HECTORITE
Finely ground, white, sodium hectorite clay exhibiting high cation exchange capacity. Used as a binder and plasticizer in wall and floor tile. Exhibits excellent increases in green strength.
Specific Gravity: 2.5
pH (5% dispersion): 9.5-10.5
C.E.C. (meq/100g): 100
Dry Brightness (Green Filter): 70
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 2380cps
Out Bound Links
- (Typecodes)
1: CLO - Clay Other
- (MDT - Member)
North America
The decision about what materials to include in th... - (MDT - Member)
Australia
We are working on this database and would apprecia... - (MDT - Member)
New Zealand
We are working on this database and would apprecia...
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="vol353cer Hectorite" descrip="FINE GROUND SODIUM HECTORITE" searchkey="" loi="0.00" casnumber="12173-47-6">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="6.740" tolerance=""/>
<oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="U" percent="1.500" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="19.000" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="U" percent="0.730" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="2.350" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.270" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.810" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.400" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.550" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="LOI" name="Loss on Ignition" percent="20.600" tolerance=""/>
</volatiles>
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|