Vansil W WollastoniteCalcium metasilicate
A white nonmetallic, natural mineral identified chemically as calcium metasilicate, CaSiO3. It is used in ceramic wall and floor tile, in glazes, and in frits for glazes and enamels. It also finds use in glaze and body stains, in bonds for vitrified grinding wheels, in electrical insulators, and as an auxiliary flux. W-10 is 200 mesh, W-20 is 325 mesh, W-C-1 and DFSP are crushed. Out Bound Links
XML for Import into INSIGHT<?xml version="1.0" encoding="UTF-8"?> <material name="Vansil W Wollastonite" descrip="Calcium metasilicate" searchkey="W-10, W-20, W-C-1" loi="0.00" casnumber="9056-30-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="44.050" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="1.480" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="0.210" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.750" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.060" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.250" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.010" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="2.180" tolerance=""/> </volatiles> </material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
Imports many file formats
Perfect for Education
|
|
Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved |
|
INSIGHT is ceramic chemistry |