Triuranium Octaoxide

Formula: U3O8
Alternate Names: Yellowcake, Uranium Oxide

OxideAnalysisFormula
U3O8100.00%1.000
Oxide Weight842.00
Formula Weight842.00
Enter the formula and formula weight directly into the Insight MDT dialog (since it records materials as formulas).
Enter the analysis into an Insight recipe and enter the LOI using Override Calculated LOI (in the Calc menu). It will calculate the formula.

The most stable form of uranium and the one found in nature.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Triuranium Octaoxide" descrip="" searchkey="Yellowcake, Uranium Oxide" loi="0.00" casnumber="1344-59-8"> <oxides> <oxide symbol="U3O8" name="Uranium Oxide" status="" percent="100.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()

0