Stain (pink/coral)
Coral/Pink Stains (ZrFe, ZrSiFe)
Color Range
-----------
Coral pink to pink shades.
Specific Gravity: 4.25-4.75
----------------
Stability/Kiln Atmosphere
-------------------------
Excellent in all types of glazes at temperatures up to over 1300C. The most stable of the known pink ceramic stains.
Compatibility
-------------
Suitable for blending with most other types of ceramic colors. Extensively used in blends with either zircon-vanadium blue, zircon-praseodymium yellow or tin-vanadium yellow to produce stable intermediate shades.
Cost
----
Moderate.
Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.
Suitable for all types of glazes. Best results are obtained with leadless or low-lead glazes having low alkali contents. Zircon opacifiers are preferred as they help prevent solution of the stain. This system is non-metameric and therefore minimizes the effects of different lighting conditions.
derglaze Color: Owing to great stability, may be used for all methods of underglaze decoration.
See ZrFe Out Bound Links
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="Stain (pink/coral)" descrip="Coral/Pink Stains (ZrFe, ZrSiFe)" searchkey="" loi="0.00" casnumber="n/a">
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|