Silica Yuba

GROUND SILICA FLOUR

Chemistry %

K2O0.01
Al2O30.06
SiO299.86
Fe2O30.02
 

Volatiles %

LOI0.05

Sieve analysis: YubaSil 140# 200# 200F# 300# 325# 325P
------------------------------------------------
Retain on US 60 t
80 t t
100 t t t t t
140 15 5 1 1 t t
200 28 8 4 2 2 t t
270 17 9 4 7 3 1 1
325 23 11 14 8 4 4 2

Bulking Value, gals/lb: .046
Apparent Density (dry uncompacted) 90.6 lbs/cubic foot
pH (37.5% suspension): 6.5
Oil Absorption ASTM D-1483: 20 lbs/100 lbs pigment
Specific Surface Area: 1.05 square meters per gram
G.E. Brightness: 86-88
Specific Gravity: 2.65
Porosity: Non-porous


Out Bound Links

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Silica Yuba" descrip="GROUND SILICA FLOUR" searchkey="" loi="0.05" casnumber="7631-86-9"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.010" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.060" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="U" percent="99.860" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.020" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.050" tolerance=""/> </volatiles> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()