Pyrophyl R-2253Pyrophyllite
The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications. The products have shown to be excellent refractory components in foundry mold and core wash formulations. They also perform in electrical porcelain, technical ceramics and structural clay coatings. Out Bound Links
In Bound Links
XML for Import into INSIGHT<?xml version="1.0" encoding="UTF-8"?> <material name="Pyrophyl R-2253" descrip="Pyrophyllite" searchkey="" loi="2.80" casnumber="12269-78-2"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="20.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="75.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="2.800" tolerance=""/> </volatiles> </material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
Imports many file formats
Perfect for Education
|
|
Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved |
|
INSIGHT is ceramic chemistry |