Pyrofrac 1004
| DENS - Density (Specific Gravity) |
2.6 |
| SADR - Sieve Analysis Dry |
+20 mesh: 0.5
+50 mesh: 3.5
+70 mesh: 3.0
+100 mesh: 5.0
+200 mesh: 18.0
+325 mesh: 45.0 |
| PCE - Pyrometric Cone Equivalent |
20 |
| BDLB - Bulk Density lbs/cu. ft. (Packed) |
65 |
Used in structural clay coatings, refractory formulations, whiteware ceramics, art pottery to
increase refractoriness, reduce shrinkage, and widen firing range.
This material is made by crushing & screening of selectively mined andalusite/pyrophyllite/sericite ores
with heavy media separation.
Out Bound Links
- (Materials - Related)
Andalusite - Al2O3.SiO2
Chiastolite
- (Materials - Related)
Seriphyl
- (Materials - Related)
Pyrophyllite - Al2O3.4SiO2.H2O - A Soft Hydrous Aluminum Silicate
Pyrophillite
- (Materials - Related)
Alkatrol - Andalusite/pyrophyllite/sericite
In Bound Links
- (Materials - Name Brand of)
Pyrofrac - Pyrophyllite/Andalusite
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="Pyrofrac 1004" descrip="" searchkey="" loi="0.00" casnumber="12269-78-2">
<oxides>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.450" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.450" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="15.300" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="76.700" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.000" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="H2O" name="Water" percent="5.700" tolerance=""/>
</volatiles>
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|