Plainsman Troy Clay

Kaolin, Halloysite

Chemistry %

CaO0.21
MgO0.18
K2O0.64
Na2O0.05
P2O50.04
TiO21.17
Al2O332.70
SiO248.39
Fe2O31.04
MnO0.00
 

Volatiles %

LOI14.49

A material very similar to Pioneer Kaolin from Dry Branch Kaolin Co. It is classified as halloysite, which should mean that it would have a very high comparative fired shrinkage. However, its physical properties do not indicate it is significantly different than a normal kaolin.

This material is available in bulk raw or powdered to 100 mesh.

Trace Elements:
Ba 380 ppm
Sr 28 ppm
Y 48 ppm
Sc 23 ppm
Zr 350 ppm
Be 2 ppm
V 116 ppm


Out Bound Links

  • (Materials - Parent) Kaolin - Al2O3.2SiO2 or Al2Si2O5(OH)4 - Hydrated alumina silicate, Pure clay mineral

    China Clay

  • (Typecodes) 1: KAO - Kaolin
  • (Minerals - Parent mineral) Halloysite

    A clay mineral very similar to kaolin in firing an...

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Plainsman Troy Clay" descrip="Kaolin, Halloysite" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.210" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.180" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.640" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.050" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.040" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.170" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="32.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.390" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.040" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.005" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="14.490" tolerance=""/> </volatiles> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()