Plainsman Fireclay
Plainsman Fireclay
A buff firing, medium plasticity, slightly toothed fireclay. Ideally suited as a refractory agent to reduce body maturity, yet not adversely affect its working and drying properties, or overly darken its fired color.
This material is good substitute for the popular but discontinued AP Green Missouri Fireclay. It fires to a similar color and is a bit more refractory.
Fireclays are often inexpensive and thus coarsely (or even erratically ground). They are implicated in lime-popping. Fireclay should be ground to at least 30 mesh to eliminate this problem.
Out Bound Links
In Bound Links
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="Plainsman Fireclay" descrip="Plainsman Fireclay" searchkey="PFC" loi="0.00" casnumber="70694-09-6">
<oxides>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.100" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.000" tolerance=""/>
<oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.020" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.700" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="27.000" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.100" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.000" tolerance=""/>
<oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.010" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="LOI" name="Loss on Ignition" percent="8.700" tolerance=""/>
</volatiles>
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|