Pemco Frit Pb-1492

LEADED FRIT

Chemistry %

CaO8.90
Li2O0.70
MgO1.40
K2O1.60
Na2O2.00
SrO3.60
PbO14.10
Al2O36.20
B2O39.30
SiO252.20
COLE - Co-efficient of Linear Expansion 6.7 x 10-6 (50-450C)
MLPT - Melting Point (MP) 1500F
MLRG - Melting Range (C) 1470-1580F
IFP - I.F.P. (celsius) 610C

Particularly suited for wollastonite bodies in a range of Cone 04 through Cone 2. Can be used alone or in partially-fritted glazes.


Out Bound Links

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1492" descrip="LEADED FRIT" searchkey="Frit Pb1492" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="8.900" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="U" percent="0.700" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="1.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="U" percent="1.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="2.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="U" percent="3.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="U" percent="14.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="9.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.200" tolerance=""/> </oxides> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()