Pemco Frit Pb-106

Lead high calcium frit for dinnerware glazes

Chemistry %

CaO18.00
K2O1.60
Na2O1.80
PbO10.10
Al2O33.40
B2O319.50
SiO245.60
COLE - Co-efficient of Linear Expansion 7.80
MLPT - Melting Point (MP) 1680F
MLRG - Melting Range (C) 1650-1730F
IFP - I.F.P. (celsius) 658C

Out Bound Links

  • (Materials - Alternative) Pemco Frit P-25 - Leadless alkaline fluorine frit, use for cone 06-02

    Pemco 25, Pemco Frit 25

  • (Materials - Alternative) Hommel Frit 25 - Leadless Sodium Boron Frit
  • (Materials - Parent) Frit - Frit master

    Ceramic Frits

  • (Typecodes) 1: FRL - Leaded Frit
  • (Typecodes - Type) 1: FRT - Frit

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-106" descrip="Lead high calcium frit for dinnerware glazes" searchkey="Frit Pb106" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="18.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="U" percent="1.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="1.800" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="U" percent="10.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="19.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.600" tolerance=""/> </oxides> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()