Pechiney Alumina
Abrasives & Refractories
AC44 AC45 AC46 AR12 SH500 SH950
Physical Properties: ------------------------------------
Ultimate Crystal Size, microns: 3-4 3-4 3-4
BET surface area, sq m per g: 0.6 0.6 0.4 13
Blaine surface area, sq cm/g: 5200 5200 4400
LOI, 20C-1000C: 0.13 0.12 0.12 0.5
Out Bound Links
- (Materials - Parent)
Alumina Hydrate - Al2O3.3H2O
Alum Hydrate, Alumina Trihydrate, Hydrated Alumina, Alpha Aluminum Trihydroxide, Gibbsite
- (Materials - Parent)
Alumina - Al2O3
Aluminum Oxide
- (Typecodes)
1: ALM - Alumina
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="Pechiney Alumina" descrip="" searchkey="" loi="0.00" casnumber="">
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|