Chemistry %

CaO0.30
MgO30.48
Na2O0.02
Al2O31.65
SiO260.10
Fe2O30.45
MnO0.00
 

Volatiles %

H2O0.55
LOI6.98

Out Bound Links

  • (Materials - Parent) Talc - Mg3Si4O6 or 3MgO.4SiO2.H2O

    Magnesium Silicate, Steatite, French Chalk, Hydrated talc

  • (Typecodes) 1: FLS - Flux Source
  • (MDT - Member) Asia

    All of Asia including Turkey, Russia, Indosnesia, ...

  • (MDT - Member) Africa

    All of continental Africa. We are working on this ...

  • (Hazards - General) Talc Hazards Overview
    Hazards of this material in the ceramic industry a...

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Noor Talc" descrip="Talc" searchkey="One Talc, Egyptian Talc" loi="0.00" casnumber="14807-96-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="30.480" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="0.020" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.650" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.450" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.000" tolerance=""/> </oxides> <volatiles> <volatile symbol="H2O" name="Water" percent="0.550" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="6.980" tolerance=""/> </volatiles> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()