Digitalfire Ceramic Materials Database

Logged in as Level 2 access: Logout


Nickel Carbonate

Formula: NiCO3

Chemistry %

NiO62.93
 

Volatiles %

CO237.07

Used as a colorant in ceramic glazes and glasses.
Watch out for glaze blistering, this generates a lot of gases of decomposition.


Out Bound Links

  • (URLs) Nickel Carbonate at ilo.org
    http://www.ilo.org/public/english/protection/safew...
  • (Materials - Related) Nickel Oxide Black - Ni2O3

    Ni2O3, Nickelic Oxide, Nickel sesquioxide, Nickel (II) oxide

  • (Hazards - General) Nickel Compounds Toxicity
    The ceramic toxicity of nickel in its various form...
  • (Typecodes) 1: GNM - Generic Material
  • (Typecodes) 1: CLT - Colorant
  • (MDT - Member) North America

    The decision about what materials to include in th...

  • (MDT - Member) Europe

    Countries of Eastern Europe and former Soviet Unio...

  • (MDT - Member) Asia

    All of Asia including Turkey, Russia, Indosnesia, ...

  • (MDT - Member) Australia

    We are working on this database and would apprecia...

  • (MDT - Member) Latin and South America

    Latin America and South America. We are working on...

  • (MDT - Member) Africa

    All of continental Africa. We are working on this ...

  • (MDT - Member) Ron Roy

    This is the traditional Ron Roy materials file. He...

  • (MDT - Member) Crystal Glazes

    These materials are specially defined for makers o...

  • (MDT - Member) New Zealand

    We are working on this database and would apprecia...

In Bound Links

  • (Materials - Unspecified) Nickel Oxide Green - NiO

    NiO, Nickelous oxide, Green Nickel Oxide

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Nickel Carbonate" descrip="" searchkey="NiCO3" loi="0.00" casnumber="65405-96-1"> <oxides> <oxide symbol="NiO" name="Nickel Oxide" status="" percent="62.930" tolerance=""/> </oxides> <volatiles> <volatile symbol="CO2" name="Carbon Dioxide" percent="37.070" tolerance=""/> </volatiles> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()