Digitalfire Ceramic Materials Database

Logged in as Level 2 access: Logout


Mineral Colloid BP

Targetted at waterbased paints and coatings, Mineral Colloid® BP is a high purity montmorillonite refined from carefully selected natural bentonite.

Mineral Colloid BP exhibits excellent thixotropic properties , enhancing suspension, stability and viscosity control

The use of Mineral Colloid BP increases sag resistance and reduces syneresis and settling.

Mineral Colloid BP is totally inorganic and therefore not susceptible to enzyme attack.

Mineral Colloid BP is not affected by high shear nor high temperatures during manufacturing. Mineral Colloid®BP can be sheared repeatedly.

The type of rheology Mineral Colloid®BP exhibits lends itself to excellent spray atomization.

Low levels of Mineral Colloid BP are needed in a paint system because of its high gel strength.


Out Bound Links

In Bound Links

  • (Materials - Related) Bentolite L - White Firing Bentonite

    Bentolite

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Mineral Colloid BP" descrip="" searchkey="" loi="0.00" casnumber=""> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()