Manganese Carbonate
Formula: MnCO3
| DENS - Density (Specific Gravity) |
3.60 |
| MLPT - Melting Point (MP) |
300C D |
Mechanisms
Glaze Color - Purple In leaded glazes manganese carbonate can produce purple tinged with brown.
Glaze Color - Blue-Purple In an alkaline glaze, manganese carbonate can produce blue-purple and plum colors.
Out Bound Links
- (Materials - Unspecified)
Manganese Granular - MnO2 - Manganese, Granular Pyrolusite
Granular Manganese
- (Materials - Unspecified)
Manganese Dioxide - MnO2
Mno2, Pyrolusite, Manganese(IV) oxide
- (Materials - Unspecified)
Manganese Oxide - MnO - Pyrolusite, Manganese (black)
MnO, Manganese(II) Oxide
- (Hazards)
Manganese in Clay Bodies
Hazards of these materials in ceramic glazes and c... - (Typecodes)
1: GNM - Generic Material
- (Typecodes)
1: CLT - Colorant
- (Temperatures - Unspecified)
Manganese Carbonate decomposed to MnO (200C-?)
Release of carbon dioxide to give manganese(II) ox... - (MDT - Member)
Europe
Countries of Eastern Europe and former Soviet Unio... - (MDT - Member)
Australia
We are working on this database and would apprecia... - (MDT - Member)
Asia
All of Asia including Turkey, Russia, Indosnesia, ... - (MDT - Member)
Africa
All of continental Africa. We are working on this ... - (MDT - Member)
Latin and South America
Latin America and South America. We are working on... - (MDT - Member)
New Zealand
We are working on this database and would apprecia... - (MDT - Member)
North America
The decision about what materials to include in th... - (MDT - Member)
UK
We are working on this database and would apprecia... - (MDT - Member)
Crystal Glazes
These materials are specially defined for makers o...
In Bound Links
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="Manganese Carbonate" descrip="" searchkey="" loi="0.00" casnumber="598-62-9">
<oxides>
<oxide symbol="MnO" name="Manganous Oxide" status="" percent="61.620" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="CO2" name="Carbon Dioxide" percent="38.380" tolerance=""/>
</volatiles>
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|