Hyplas 71 Ball ClayDevon medium strength low iron ball clay
LOI estimated Out Bound Links
XML for Import into INSIGHT<?xml version="1.0" encoding="UTF-8"?> <material name="Hyplas 71 Ball Clay" descrip="Devon medium strength low iron ball clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.800" tolerance=".4"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.600" tolerance=".2"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.750" tolerance="2.25"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.500" tolerance="2.5"/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.800" tolerance=".2"/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.200" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="5.300" tolerance=""/> </volatiles> </material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
Imports many file formats
Perfect for Education
|
|
Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved |
|
INSIGHT is ceramic chemistry |