Hommel Frit 90
Leadless Frit
| COLE - Co-efficient of Linear Expansion |
7.70 |
| MLPT - Melting Point (MP) |
1550F |
| MLRG - Melting Range (C) |
1550F |
Out Bound Links
- (Materials - Substitute)
Hommel Frit 378A
Frit 378-A
- (Materials - Substitute)
Pemco Frit P-311 - Calcium borosilicate frit for partially fritted dinnerware glazes
Frit 311, Frit P311
- (Materials - Parent)
Frit - Frit master
Ceramic Frits
- (Typecodes - Type)
1: FRT - Frit
In Bound Links
- (Materials - Substitute)
Ferro Frit 3124 - Leadless high calcium borosilicate frit
F3124
- (Materials - Substitute)
Fusion Frit F-19 - Boro Calcium Dinnerware Frit
Frit F19, F19 Fusion
- (Materials - Alternative)
General Frit GF-113 - Leadless High Boron/lime Glaze Frit
Frit 113, Frit GF113
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="Hommel Frit 90" descrip="Leadless Frit" searchkey="" loi="0.00" casnumber="65997-18-4">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="13.970" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="0.760" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="U" percent="0.410" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="6.330" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.750" tolerance=""/>
<oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.920" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.860" tolerance=""/>
</oxides>
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|