Hommel Frit 389

Strontium calcium silicate frit

Chemistry %

CaO9.73
Li2O0.41
MgO0.72
K2O2.96
Na2O2.79
SrO4.43
Al2O312.12
B2O35.26
SiO261.58
COLE - Co-efficient of Linear Expansion 7.30
MLPT - Melting Point (MP) 1750F

Out Bound Links

  • (Materials - Parent) Frit - Frit master

    Ceramic Frits

  • (Materials - Parent) Frit - Frit master

    Ceramic Frits

  • (Typecodes - Type) 1: FRT - Frit

In Bound Links

  • (Materials - Substitute) Ferro Frit 3292 - For Cone 3-5 Sanitary Ware Glazes

    F3292

  • (Materials - Substitute) Fusion Frit F-134 - Strontium frit base for cone 5-6 glazes

    F134 Fusion

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 389" descrip="Strontium calcium silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="U" percent="9.730" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="U" percent="0.410" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="U" percent="0.720" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="U" percent="2.960" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="U" percent="2.790" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="U" percent="4.430" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.120" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.260" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.580" tolerance=""/> </oxides> </material>
The future of ceramic recipe, material and physical testing record keeping is here.
Watch the video or sign-up at http://insight-live.com.

Maintain your recipe database on-line

  • Login to a private account or work with others in a group account (e.g. university).
  • Nothing to install (access it using your web browser). It is always the latest version.
  • Easy to import your existing data.
  • As many side-by-side recipes as you want.
  • Many ways to search and classify glaze and body recipes.
  • Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
  • Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
  • Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
  • Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
  • Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
  • It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).

Imports many file formats

  • Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
  • Assign a batch number to imports, and later search by batch.
  • Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
  • Prepend character sequences to glaze recipe names during import.
  • Import the pictures and pair them to their corresponding records automatically.
  • One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
  • Export and import individual glaze recipes as text or XML.

Perfect for Education

  • Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
  • Students already have internet connected devices, computers are not even needed in the class.
  • The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..



Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008 http://digitalfire.com, All Rights Reserved
Get a free INSIGHT software trial

INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. ()