FT-HSF Clay
Westerwald, Germany - Plastic Clay
Raw Color - CREAM
Particle Size (e.s.d.)
125 microns - 1.7
63 microns - 5.0
20 microns - 90
2 microns - 70
.5 microns - 53
Modulus of Rupture at 110C
Mn/M2 - 3.7
lbf/in2 - 540
Water Absorption
1120C - 4.5
1220C - 0.50
Shrinkage Dry to Fired
1120C - 6.1
1220C - 9.0
Refractoriness
Cone - 28, 1630C
Plastic Index - 690
PF NO. - 33.3
Out Bound Links
XML for Import into INSIGHT
<?xml version="1.0" encoding="UTF-8"?>
<material name="FT-HSF Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="6.50" casnumber="70694-09-6">
<oxides>
<oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/>
<oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/>
<oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.200" tolerance=""/>
<oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/>
<oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.500" tolerance=""/>
<oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.700" tolerance=""/>
<oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.100" tolerance=""/>
<oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.700" tolerance=""/>
</oxides>
<volatiles>
<volatile symbol="C" name="Carbon" percent="0.200" tolerance=""/>
<volatile symbol="LOI" name="Loss on Ignition" percent="6.300" tolerance=""/>
</volatiles>
</material> |
The future of ceramic recipe, material and physical testing record keeping is here.
Maintain your recipe database on-line
- Login to a private account or work with others in a group account (e.g. university).
- Nothing to install (access it using your web browser). It is always the latest version.
- Easy to import your existing data.
- As many side-by-side recipes as you want.
- Many ways to search and classify glaze and body recipes.
- Glaze and body recipes are robust, with units-of-measure, unlimited pictures with individual titles and descriptions.
- Add variations to a recipe; each with its own pictures, descriptions and name/code-number extensions.
- Recipes can link to typecodes, projects and firing schedules (all managed in their own areas).
- Standard reports and mix ticket reports with last-minute-totalling; variations report as if they are a complete recipe.
- Video tutorials, help system, contact form on every page, dedicated messaging and support ticket systems.
- It is an industrial-strength database system (unlimited capacity, fast, reliable, scalable).
Imports many file formats
- Glaze recipe formats supported: HyperGlaze, GlazeGhem, GlazeMaster, Matrix, INSIGHT XML recipes (single and multiple), INSIGHT SQLite DB files.
- Assign a batch number to imports, and later search by batch.
- Assign multiple typecodes to imported glaze and body batches (to classify) and search on these later.
- Prepend character sequences to glaze recipe names during import.
- Import the pictures and pair them to their corresponding records automatically.
- One click to automatically export the database to an SQLite DB database file and download it (for use with desktop INSIGHT or just as a backup).
- Export and import individual glaze recipes as text or XML.
Perfect for Education
- Ceramic study programs can now accumulate material, recipe and testing data year-after-year, students can login and together build a valuable ceramic glaze and body knowledge resource.
- Students already have internet connected devices, computers are not even needed in the class.
- The Reference Manager gives you quick access to the Digitalfire Ceramic Reference Database.
Learn more..
|